* Not suitable for mechanical parts. | * Not suitable for mechanical parts. | ||
==== Variants ==== | ==== Variants ==== | ||
- | PVA filaments only come in natural coloration and do not contain fill additives such as glass fibers. | + | PVA filaments only come in natural coloration and does not contain fill additives such as glass fibers. |
Line 16: | Line 16: | ||
These numbers are provided as a baseline, and **need** adjustment and calibration for your specific printer/ | These numbers are provided as a baseline, and **need** adjustment and calibration for your specific printer/ | ||
- | ^ Variant | + | ^ Variant |
|PVA |220 |60 |Not required | |PVA |220 |60 |Not required | ||
==== Other notes ==== | ==== Other notes ==== | ||
- | This page is a stub. | + | It is ideal to print PVA from a dry box with a bowden tube and a fresh silica gel packet to delay the ingress of moisture into the material. |
+ | |||
+ | If PVA filament soaks too much moisture, upon printing the material will turn white out of the hotend and loud crackling can be heard as the moisture evaporates from the material. | ||
+ | |||
+ | Additionally if the filament has soaked too much moisture, for example the spool was left unattended to outside of a dry box for a week then hydrolysis will degrade the material substantially and individual strands of the spool can fuse together upon attempting to dry it. | ||
+ | |||
+ | PVA becomes flexible when it is wet. | ||
+ | |||
+ | Print at slow speeds for best results. | ||
+ | |||
+ | For optimal bed adhesion it is recommended to apply a thin layer of glue stick. |